High quality 99.99% Scandium Black Powder with Best Price for various superalloys
Quick Details Port: shanghai Payment Terms: L/C,D/A,D/P,T/T,Western Union,MoneyGram Supply Ability: 10000.0 Kilogram/Kilograms per Month Content(percent): 99.9% Boiling Point: 2836 °C Composition: Sc CAS No: 7440-20-2 Stability: Fairly stable in air Grade: metal MW: 44.96 Multilingual: Scandium Metall, Metal De Scandium, Metal Del Scandium Density: 2.99 g/cm3 Appearance: Silvery lump pieces or other solid form Formula: Sc Product Type: Rare Earth Metal Product name: Scandium Metal Application: various superalloys Melting point: 1540 °C Packaging Detail: 25kg net per bag,outer woven bags with inner plastic lining